WE 20CV Subjugator edge retention testing. Has thier top tier steel improved any or is it average?
Published: 2 years ago
WE 20CV Subjugator edge retention testing. Has thier 30CV heat treat improved or is it just mediocre? This had already been sharpened so it's just the normal 3rd and 4th edge testing. I'll cover the sharpening as well.
WE Subjugator 20CV hardness 60.5 rc
Outpost 76 Patreon